Boya öncesi don kaplama olarak uygulanabilen üstün nitelikli beyaz çimento esaslı ısı değişikliklerine suya ve dona dayanıklı kolay uygulanabilen tekstüre görünüm sağlayan yüzey düzeltme sıvasıdır.
Daha Fazla Bilgi Alın İletişime GeçinBoya öncesi don kaplama olarak uygulanabilen üstün nitelikli beyaz çimento esaslı ısı değişikliklerine suya ve dona dayanıklı kolay uygulanabilen tekstüre görünüm sağlayan yüzey düzeltme sıvasıdır.
Color | White |
Package | 25 Kg craft bags |
Water mixing ratio | 6 - 6,5 Lt |
Application degree | +5C & +30C |
Mixture self life | 3 Hour |
Application Thickness | 2-10 mm |
Caking period | < 20 dk |
Consumption | 4-6 Kg/m2 |
Opening period of traffic | 24 - 48 Hour |
Storage | In original package 12 months maz 10 line |
Resistance against hot | -30C + 80C |
Sticking strenght | >0,2 N/mm2 |
It is used on horizontal and vertical surfaces indoors and outdoors.
It is used for bonding thermal insulation coating plates on cement-based surfaces, gas concrete, pumice and brick surfaces.
It is not applied on wooden, metal and PVC surfaces.
The surface should be clean and sound, if any, dust, oil, dirt or materials that prevent adhesion should be removed from the surface, mortar, paint, cement residues, etc. should be removed. items should be scraped.
After surface cleaning, 1 coat of FILM PRIMER liquid product should be applied to the surface with a brush and left to dry for 1-2 hours in order for the adhesive to adhere better to the surface and to adhere the dust on the surface, if any, and to balance the water absorbency of the surface.
Depth 2cm. Surface defects exceeding more than 1,500 should be repaired with ÜSTÜN REPAIR 1 day before, after cleaning and priming before.
6-6.5 Lt. into a clean and round shaped container. put clean water and 25 Kg. Add the powder product slowly and mix until a homogeneous appearance is formed, without leaving any lumps.
Mix with a low speed (400dv/min) electric mixer.
Let the mixture rest for 10 minutes and mix again for another 30 seconds and use
Care should be taken to ensure that the ambient and ground temperature to be applied is between +5C and +30C.
It is applied to the heat insulation boards on smooth surfaces of the mixed mortar screed and balance, by scanning the entire surface of the surface with a toothed steel comb trowel.
If there are elevation differences on the application surfaces, this level difference should be at most 1 cm under the 2-meter gauge and the heat insulation plates should be adhered by point bonding method.
In the point bonding method, adhesive must be applied along all the edges of the thermal insulation plates, and point adhesive mortar must be applied to the center and corner areas of the plates.
After bonding, the level of the plates should be checked with a large surface gauge.
Mechanical anchoring should be done at least 24 hours after bonding.
Do not work in extreme windy and sunny weather in outdoor applications.
Add extra water, cement, etc. to the mix. Do not make additions.
Never apply on frozen, dusty and dirty surfaces.